Hi Guys,

 

I have a Shine V2 front bumper on my zed, it was painted a few months ago by a decent body shop but after a few weeks I started noticing small cracks in the body work.

 

IMG00097-20100830-1428.jpg

 

IMG00098-20100830-1428.jpg

 

IMG00099-20100830-1428.jpg

 

Now I know the Shine bumper is made from FG but I wouldnt expect it to break up so quickly...this might have something to do with my zed being quite low to the floor. Is there a special primer that I can get which will stop this from happening? Someone suggesting a flexible plastic primer.

 

Thoughts?

Link to comment
Share on other sites

Yup your right mate most companys should use this primer on bumper, helps with small bumper etc. Think they call it plastersize or somthing but the bodyshop should know this. I would take it back if you havent hit anything..

 

Alex

Link to comment
Share on other sites

Thanks guys....guess I wont be using that body shop again! My zed is quite low and maybe having a FG front end isnt the best idea.

 

I did have the badge smoothed out which has made the middle of the bumper fairly rigid and left the sides where thee cracks are with some flex...I assume thats probably contributed to the problem aswell.

 

I will have to find someone better to repaint the front end when it goes back to the body shop.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...